55% Min Ferro Molybdenum Description

 

55% Min Ferromolybdenum is used in the production of ferrous alloys. Ferromolybdenum is selected by various industrial sectors based on its molybdenum content for use in the production of military machinery, machine tools and equipment, load-bearing elements, rotary drills and pipes for oil refining. It is also used in vehicles, including cars, trucks, and trains. Ferromolybdenum is added to stainless steel and heat-resistant steels. These products are used in a variety of installations, equipment, and systems, including refinery equipment, chemical plants, synthetic fuel plants, pumps, heat exchangers, and so on. In addition, it is added in large quantities to tool steels for use in ball and rolling mills, large drills, high-speed machining components, dies, chisels, and so on.

 

55% Min Ferro Molybdenum

 

 

The Specification Of 55% Min Ferro Molybdenum

 

Greater than or equal to 70 1,50 0.10-0.15 0,05 0,10 0,50 0,04 0,04
65-70 1,50 0.10-0.15 0,05 0,10 0,50 0,04 0,04
55-65 1,00 0,10 0,04 0,10 0,50 0,04 0,04
55-65 1,50 0,10 0,05 0,10 0,50 0,05 0,06
55-65 2,00 0,15 0,05 0,20 1,00 0,08 0,08
>55 2,00 0,10 0,05 0,15 0,50 0,04 0,04
>55 1,00 0,10 0,08 0,20 0,50 0,05 0,06
>55 1,50 0,15 0,08 0,25 1,00 0,08 0,08

 

 

55% Min Ferromolybdenum For Sale55% Min Ferromolybdenum on Request

 

 

 

A: Always a pre-production sample before mass production; Always final Inspection before shipment.

تگ های محبوب: 55% min ferro molybdenum, China 55% min ferro molybdenum manufacturers, suppliers