10-50 mm خاکستری 70 ٪ توضیحات سیلیکون فرو
Ferrosilicon is used to produce silicon, which is used to reduce metals from their oxides and remove oxides from steel and other ferrous alloys. This prevents the carbon from volatilizing from the molten steel. It is also used to produce silicon, as well as other materials that are resistant to corrosion and high temperatures. These materials are used in electric motors and transformer هسته .
ما به پایداری اعتقاد داریم.
![]()
مشخصات 10-50 mm خاکستری 70 ٪ سیلیکون فرو
| درجه | کسر جرم ، ٪ | |||||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| si | C | S | P | با هم | منگنه | کلوچه | ||||||||
| کمتر از | بیش از | |||||||||||||
| FESI75 | 74,0 - 80,0 | 0,1 | 0,02 | 0,04 | 3,0 | 0,4 | 0,3 | |||||||
| FESI70 | 68,0 - 74,0 | 0,1 | 0,02 | 0,04 | 2,0 | 0,4 | 0,4 | |||||||
| FESI65 | 63,0 - 68,0 | 0,1 | 0,02 | 0,05 | 2,5 | 0,4 | 0,4 | |||||||
| FESI45 | 41,0 - 47,0 | 0,2 | 0,02 | 0,05 | 2,0 | 1,0 | 0,5 | |||||||
کارخانه ما
![]()
10-50 mm خاکستری 70 ٪ تأمین کنندگان Ferrosilicon
مشتریان بازدید می کنند
![]()
10-50 mm خاکستری 70 ٪ تولید کنندگان Ferrosilicon
پرسش
س: آیا برای نمونه ها شارژ می کنید؟
پاسخ: مطابق با سیاست شرکت ما ، نمونه ها رایگان هستند ، ما فقط هزینه حمل و نقل. را پرداخت می کنیم و هزینه حمل و نقل را در طول سفارش بعدی برمی گردانیم .
س: آیا می توانید مطابق با طراحی مشتری تولید کنید؟
پاسخ: مطمئناً ، ما یک تولید کننده حرفه ای هستیم . ما می دانیم که نیازهای هر مشتری منحصر به فرد است . قابلیت های تولید انعطاف پذیر ما به ما امکان می دهد محصولات را متناسب با الزامات خاص .}
س: ظرفیت تولید و تاریخ تحویل شما چیست؟
پاسخ: 3000 متر در ماه و در 20 روز پس از پرداخت . ارسال شد
س: آیا قیمت قابل مذاکره است؟
پاسخ: بله ، لطفاً در صورت داشتن هرگونه سؤال . و برای مشتریانی که می خواهند بازار را بزرگ کنند ، در هر زمان با ما تماس بگیرید ، ما تمام تلاش خود را برای پشتیبانی از آنها انجام خواهیم داد. 1 {1}
تگ های محبوب: 10-50 mm خاکستری 70 ٪ فروم سیلیکون ، چین 10-50 mm خاکستری 70 ٪ تولید کنندگان سیلیکون Ferro ، تأمین کنندگان